006068
Photograph 006068 Second World War, 1939-1945OWING TO THE TERRIFIC HEAT TO WHICH THE POTS ARE SUBJECTED, THEIR COMPOSITION MUST BE PERFECT. THIS PICTURE SHOWS A POT THAT COULD NOT STAND UP TO THE INTENSE HEAT. (NEGATIVE BY E.L. CRANSTONE).

The Australian War Memorial Collection. Test site
TWO EXAMPLES OF GLASS. THE LEFT SHOWS GLASS THAT HAS ABSORBED IRON FROM THE POT WHILE THE ONE ON THE RIGHT SHOWS PERFECT QUALITY. (NEGATIVE BY E.L. CRANSTONE).
OWING TO THE TERRIFIC HEAT TO WHICH THE POTS ARE SUBJECTED, THEIR COMPOSITION MUST BE PERFECT. THIS PICTURE SHOWS A POT THAT COULD NOT STAND UP TO THE INTENSE HEAT. (NEGATIVE BY E.L. CRANSTONE).

THE GLASS MIXTURE IS CAREFULLY WEIGHED OUT, PRIOR TO BEING PLACED IN THE POT FOR MELTING. MR. G.M. WILLIS. (NEGATIVE BY E.L. CRANSTONE).

CLAY POTS ARE USED TO MAKE THE GLASS. THIS EXPERIMENTAL POT IS QUITE SMALL. POTS USED ULTIMATELY WILL BE SEVERAL FEET IN DIAMETER. (NEGATIVE BY E.L. CRANSTONE).

PROFESSOR HARTUNG PLACES A POT IN THE FRESHLY LIGHTED FURNACE. THE POT MUST BE HEATED SLOWLY TO PREVENT CRACKING. THIS TAKES AS LONG AS 8 HOURS. (NEGATIVE BY E.L. CRANSTONE).

AFTER BEING COOLED SLOWLY OVER NIGHT, THE POT IS TAKEN OUT AND BROKEN APART. MR. G. AMPT. SENIOR LECTURER IN ANALYTICAL CHEMISTRY. (NEGATIVE BY E.L. CRANSTONE).

THE FINISHED OPTICAL GLASS. (NEGATIVE BY E.L. CRANSTONE).